Here "DD Fiberglass" shows fiberglass mesh weaving defects in appearance. Fiberglass mesh appearance defects also influence fiberglass quanlity a lot. Let us see what defects appear in fiberglass mesh fabrics.
- Broken end;
- Loose, tight end;
- Mixed end, mixed filling;
- include double ends, wrong tex number, wrong plies number, misdraw;
- Broken picks, sloughed-off weft;
- Double pick;
- Grin;
- Filling bar;
- Abutting joint;
- Hole;
- Break out;
- Foreign matter;
- Spot;
- Defective selvedge;
- Flying thread;
- Felter;
- Distortion.
These 16 defects are common fiberglass mesh defects, we should be careful in each production process to assure the quanlity.